Failure analysis of 12 mm OD SS 304 tube pertaining to instrument tapping line of nitrogen storage vessel
IR@NAL: CSIR-National Aerospace Laboratories, Bangalore
View Archive InfoField | Value | |
Title |
Failure analysis of 12 mm OD SS 304 tube pertaining to instrument tapping line of nitrogen storage vessel
|
|
Creator |
Suresh Kumar, M
Madan, M Venkataswamy, MA Sujata, M Parameswara, MA Bhaumik, SK |
|
Subject |
Aeronautics (General)
Chemistry and Materials (General) |
|
Description |
The SS304 tubing of the instrument tapping line connected to nitrogen storage vessel has failed by thick-lip rupture under Hoop stress. Evidences suggest that the failure was due to presence of defects in the tubes. The defects were identified as preexisting longitudinal cracks, typical of extrusion defects. It is recommended that the entire SS304 tubing of the instrument tapping line be changed to prevent recurrence of similar failures.
|
|
Publisher |
National Aerospace Laboratories
|
|
Date |
2005
|
|
Type |
Proj.Doc/Technical Report
NonPeerReviewed |
|
Identifier |
Suresh Kumar, M and Madan, M and Venkataswamy, MA and Sujata, M and Parameswara, MA and Bhaumik, SK (2005) Failure analysis of 12 mm OD SS 304 tube pertaining to instrument tapping line of nitrogen storage vessel. Project Report. National Aerospace Laboratories, Bangalore.
|
|
Relation |