A facile synthesis of grainy rod-like porous MgO

IR@CGCRI: CSIR-Central Glass and Ceramic Research Institute, Kolkata

View Archive Info
 
 
Field Value
 
Title A facile synthesis of grainy rod-like porous MgO
 
Creator Hazra Chowdhury, Arpita
Hazra Chowdhury, Ipsita
Naskar, Milan Kanti
 
Subject Engineering Materials
 
Description Porous magnesia (MgO) with grainy rod-like microstructure was synthesized by hydrothermal process at 180 degrees C/5 h in the presence of urea. The as-prepared particles crystallized as Mg-5(CO3)(4)(OH)(2)center dot 5H(2)O which transformed to MgO phase at 600-700 degrees C. The BET surface area, total pore volume and average pore diameter of 600 degrees C-treated sample were found to be 46 m(2) g(-1), 0.34 cm(3) g(-1) and 30.4 nm, respectively. Microstructural analysis indicated grainy rod-like microstructure (aspect ratio 10-30) in which the nanograin-like particles (20-50 nm) were assembled like architectural design. (C) 2015 Elsevier B.V. All rights reserved.
 
Publisher Elsevier
 
Date 2015-11
 
Type Article
PeerReviewed
 
Format application/pdf
 
Identifier http://cgcri.csircentral.net/2969/1/ipsita.pdf
Hazra Chowdhury, Arpita and Hazra Chowdhury, Ipsita and Naskar, Milan Kanti (2015) A facile synthesis of grainy rod-like porous MgO. Materials Letters, 158. pp. 190-193. ISSN 0167-577X
 
Relation http://cgcri.csircentral.net/2969/