Effect of fluorine substitution on sintering behaviour, mechanical and bioactivity of hydroxyapatite

IR@CGCRI: CSIR-Central Glass and Ceramic Research Institute, Kolkata

View Archive Info
 
 
Field Value
 
Title Effect of fluorine substitution on sintering behaviour, mechanical and bioactivity of hydroxyapatite
 
Creator Nasker, Purnendu
Samanta, Aniruddha
Rudra, Sudip
Sinha, Arijit
Mukhopadhyay, Anoop Kumar
Das, Mitun
 
Subject Environment and Pollution
 
Description Fluorine substituted hydroxyapatite (FAp) with different degree of fluorine (F) substitution, has been synthesized using hydrothermal synthesis method. In the present work, as synthesized powders were consolidated by sintering at 1200 degrees C in air for 1 h. The sintered specimens were characterized using Fourier transform infrared spectroscopy (FTIR) and X-ray diffraction (XRD) for phase analysis. Further, fluorine intake in the sintered specimens was evaluated using ion chromatography (IC). XRD peaks clearly showed biphasic nature of the sintered specimen. However, the sintered samples containing more than similar to 60% fluorine substitution showed no P-tricalcium phosphate (beta-TCP) phase formation. The IC results revealed that the degree of fluoridation decreased significantly in the sintered specimen compare to the respective as synthesized powders. The effect of actual fluorine content in the sintered specimens was further evaluated in terms of sinterability, surface energy, mechanical properties and in vitro cytocompatibility study. The surface energy of the sintered specimen decreased from 51.8 mN/m to 42.5 mN/m, in which degree of fluoridation varies from 0% to 110%. The in vitro cytocompatibility of the sintered specimen were carried out against mouse osteoblast cell line (MC3T3-E1). In vitro study showed that all the samples were nontoxic but cell proliferation for the samples containing more than 40% fluorine substitution became significantly low.
 
Publisher Elsevier
 
Date 2019-07
 
Type Article
PeerReviewed
 
Format application/pdf
 
Identifier http://cgcri.csircentral.net/4632/1/nasker2019.pdf
Nasker, Purnendu and Samanta, Aniruddha and Rudra, Sudip and Sinha, Arijit and Mukhopadhyay, Anoop Kumar and Das, Mitun (2019) Effect of fluorine substitution on sintering behaviour, mechanical and bioactivity of hydroxyapatite. Journal of the Mechanical Behavior of Biomedical Materials, 95. pp. 136-142. ISSN 1751-6161
 
Relation http://cgcri.csircentral.net/4632/