CSIR Central

Thermal degradation of waste plastics under non-sweeping atmosphere: Part 2: Effect of process temperature on product characteristics and their future applications

IR@CMERI: CSIR- Central Mechanical Engineering Research Institute (CMERI), Durgapur

View Archive Info
 
 
Field Value
 
Title Thermal degradation of waste plastics under non-sweeping atmosphere: Part 2: Effect of process temperature on product characteristics and their future applications
 
Creator Singh, Rohit Kumar
Ruj, Biswajit
Sadhukhan, Anup Kumar
Gupta, Parthapratim
 
Subject Thermal stability
 
Description The current energy demand and diminishing conventional fuels have forced researchers to find an alternative source of energy. Waste to energy is the current trend for converting waste materials (plastic waste) into valuable fuels. This article mainly discussed the detailed characterization of the pyrolytic products, their comparative analysis and the reaction mechanism at varying operating temperature. This article is a successor of part 1, which primarily focused on the characterization of different waste plastics, their TG analysis, the effect of reactor temperature on yield analysis in a batch reactor and their detailed degradation mechanism. Furthermore, the results presented in this article report the characterization of products at three processing temperatures of 450, 500 and 550 °C. The pyrolytic oils from all wastes excluding PS show a very low density ranging from 0.71 to 0.76 kg/m3, whereas PS pyrolytic density is reported between 0.86 and 0.88 kg/m3. The viscosity of oils increases with an increase in the processing temperature and is similar to the conventional fuels. The FTIR analysis of the products (oil & gases) obtained from HDPE, PP and mixed plastic waste (MIX) shows a large presence of alkanes and a higher presence of aromatics. PS analysis reported a large presence of aromatics (~75%). The GC-MS analysis of all pyrolytic oils from waste plastics, simulated wastes (virgin plastics) and distilled fraction of MIX pyrolysis oil is compared. The GC analysis of non-condensable gases at all processing temperature reports that MIX produce the maximum H2; HDPE, PS and MIX produces a high amounts of CH4 too. The formation of lower hydrocarbons (C5–C12) in pyrolysis oil shows a trend as MIX > PP > PS > HDPE, while for the heavier hydrocarbons (>C19) it is HDPE > PP > PS > MIX. The potential of the utilization of these products has been discussed in different sectors for future research.
 
Publisher Elsevier
 
Date 2020-05-01
 
Type Article
PeerReviewed
 
Identifier Singh, Rohit Kumar and Ruj, Biswajit and Sadhukhan, Anup Kumar and Gupta, Parthapratim (2020) Thermal degradation of waste plastics under non-sweeping atmosphere: Part 2: Effect of process temperature on product characteristics and their future applications. Journal of Environmental Management, 261 (110112).
 
Relation http://cmeri.csircentral.net/726/