Description The influence of surface mechanical attrition treatment (SMAT) on the corrosion behaviour of AISI 409 grade stainless steel in 0.6 M NaCl was studied. SMAT using 2 mm empty set 316L stainless steel (SS) balls for 15, 30 and 45 min and 5 mm empty set balls for 15 min offers a better corrosion protective ability. In contrast, treatment using 5 mm empty set balls for 30 and 45 min and by using 8 mm empty set balls for 15, 30 and 45 min, induces microstrain and defect density that results in a decrease in corrosion resistance. (C) 2010 Elsevier Ltd. All rights reserved.
 
Publisher PERGAMON-ELSEVIER SCIENCE LTDOXFORDTHE BOULEVARD, LANGFORD LANE, KIDLINGTON, OXFORD OX5 1GB, ENGLAND
 
Date 2011-09-20T11:59:52Z
2011-09-20T11:59:52Z
2010
 
Type Article
 
Identifier CORROSION SCIENCE
0010-938X
http://hdl.handle.net/123456789/11382
 
Language English