Title Failure analysis of input shaft of Maerz kiln # 6 skip drive gearbox
 
Creator Suresh Kumar, M
Sujata, M
Madan, M
Venkataswamy, MA
Banerjee, A
Bhattacharya, S
Bhaumik, SK
 
Subject Aeronautics (General)
Chemistry and Materials (General)
 
Description Evidences suggest that the input shaft has failed by stress corrosion cracking (SCC). After initiation at the keyway edges, the cracks have propagated progressively along the fillet at the change of cross section of the shaft. Once the cross section of the shaft reduced below the critical limit, it has failed by sudden torsional overload. Investigation revealed that use of improper steel with high amount of MnS was responsible for the SCC.
 
Publisher National Aerospace Laboratories
 
Date 2006
 
Type Proj.Doc/Technical Report
NonPeerReviewed
 
Identifier Suresh Kumar, M and Sujata, M and Madan, M and Venkataswamy, MA and Banerjee, A and Bhattacharya, S and Bhaumik, SK (2006) Failure analysis of input shaft of Maerz kiln # 6 skip drive gearbox. Project Report. National Aerospace Laboratories, Bangalore, India.
 
Relation http://nal-ir.nal.res.in/9712/